Before

After

Objective
Improve Surface Finish and remove build lines
| Industry | 3D Printing Plastics – Test Sample |
| Part Description | Plastic Cylinder |
| 3D Printer Technology | 3D Plastic FDM |
| Material | ABS |
| Process Technology | Surface Preparation |
| Equipment Type | Tumbling Equipment |
Bel Air Completed testing of surface finishing and coating for the customer to help them make educated decisions to best choose the printing technologies. ABS materials post processed to a molded finish.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.