Objective

Development to determine efficient build removal.

Industry3D Printed Post Process – Plastics
Part DescriptionDental Arches,
Fabrication MethodPolyjet, SLS
MaterialPlastic Medical 690
Process TechnologyRemove Build
Equipment TypeHigh energy

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.