Before Post-Processing

After Post-Processing

Objective
Improve Surface Finish for fit, form, function, and cosmetics
| Industry | 3D Print Post Process Tech – Medical |
| Part Description | Medical Parts |
| 3D Printing Technology | 3D Plastic SLA |
| Material | Verro Clear 3D Plastic Resin |
| Process Technology | Smooth & Polish Surface |
| Equipment Type | High Energy |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.