Before Post-Processing

After Post-Processing

Objective
Smooth Print Lines from FDM.
| Industry | 3D Print Post Process Tech – Plastics |
| Part Description | Stacker Parts |
| 3D Printing Technology | FDM |
| Material | Pet G & PLA |
| Process Technology | Smooth & Polish Surface |
| Equipment Type | High Energy |
Bel Air Completed testing of surface finishing and coating for the customer to help them make educated decisions to best choose the printing technologies. Pet G & PLA materials post processed to a molded finish.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.