Before Post-Processing


After Post-Processing


Objective
Process the component and determine the best method to produce an optimum surface finish.
| Industry | 3D Print Post Process Tech – Metal |
| Part Description | Thumbscrew |
| 3D Printing Technology | Metal -DMLS |
| Material | Stainless Steel |
| Process Technology | Smooth and Polish Surface + Evaluation of Different Process Methods (3D) |
| Equipment Type | High Energy |
Bel Air completed testing of surface finishing and coating for the customer to help them make educated decisions to best choose the printing technologies. DMLS materials post processed to a molded finish.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.