Before

After
Objective
Improve Surface Finish for form, function and cosmetics
| Industry | 3D Printer Plastics – Test Samples |
| Part Description | Prototype Grippers |
| 3D Printer Technology | 3D Plastic SLS |
| Material | EOS PA 1100 |
| Process Technology | Surface Preparation |
| Equipment Type | Centrifugal Disc Finisher |
In the early stages of developing production 3D AM printer equipment and materials; Bel Air was engaged by EOS to develop post processing techniques in order to feedback to the printing process for improvements to help post processing achieve traditional finishes.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.