Objective

Improve Surface Finish on Plastic Pin and improve surface finish and clarity to replica an injection molded part.

Industry3D Printing Post Process – Plastics – Test
Part DescriptionTest Pin
3D Printing Technology3D Plastic Polyjet
MaterialVero Clear
Process TechnologySurface Finish, Smooth & Polish Surface
Equipment TypeHigh energy, Centrifugal Disc Finisher

In the early stages of developing production3D, AM Printer equipment and materials, Bel Air was engaged by HP Stratasys to develop post processing techniques

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.