Before Post-Processing

After Post-Processing

Objective
Produce a polished surface finish of dental lab test pieces used for student training.
| Industry | 3D Print Post Process – Plastics – Dental |
| Part Description | polyJet Printed Acrylic Teeth |
| 3D Printing Technology | polyjetMJ |
| Material | Acrylic Resin |
| Process Technology | Smooth & Polish Surface |
| Equipment Type | High energy |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.