Before Post-Processing


After Post-Processing


Objective
Improve Surface Finish of Automotive Component for fit, form and function.
| Industry | 3D Printed Plastics – Automotive |
| Part Description | Automotive Component |
| 3D Printing Technology | MJF |
| Material | PA 1100 |
| Process Technology | Surface Finishing |
| Equipment Type | Centrifugal Disc Finsiher |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.