Before


After


Objective
Development do determine multiple process options
| Industry | 3D Printed Post Processed Part |
| Part Description | Small cartridge body |
| 3D Printing Technology | SLA |
| Material | Resin |
| Process Technology | Polish and smooth surface |
| Equipment Type | High Energy |
Need the body of the tube to be water clear. Only the body is important; the threaded portion doesn’t need any particular finish.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.