Before

After

Objective
Clean powder from build and improve surface of internal vanes, to improve function
| Industry | 3D Printed Post Process – Plastics |
| Part Description | Louver Housing |
| 3D Printer Technology | MJF |
| Material | PA 12 Nylon |
| Process Technology | De-Powder, Smooth & Polish Surface |
| Equipment Type | Centrifugal Disc Finisher |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.