Objective
Bel Air completed testing of surface finishing and coating for the customer to help them make educated decisions to best choose the printing technologies. PEKK materials post processed to a molded finish.
| Industry | 3D Printed Post Process – Plastics |
| Part Description | Sample Part |
| 3D Printer Technology | FDM |
| Material | PEKK |
| Process Technology | Smooth and Polish Surface |
| Equipment Type | Centrifugal Disc Finisher |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.