Before Post-Processing

watch component before post-processing
watch component before post-processing

After Post-Processing

Watch component after processing
Watch component after processing

Objective

Markforged  -Onyx fiber reinforced sample parts for demonstration of-Process Development to determine  multiple process options.

Industry3D Print Post Process – Plastics
Part DescriptionTest Sample
3D Printing TechnologyFFF, FDM
MaterialPlastic Onyx-Nylon composite with fiber
Process TechnologySmooth & Polish Surface
Equipment TypeMultiple Technologies

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.