Before


After


Objective
Produce a Polished Surface Finish to the feel of molded plastic.
| Industry | 3D Post Process Technology – Plastics – Consumer |
| Part Description | 3D Printed Chess Piece |
| 3D Printing Technology | SLS |
| Material | PA 1100 Nylon |
| Process Technology | Evaluation of Different Process Methods, Smooth & Polish Serface |
| Equipment Type | Centrifugal Disc Finisher |
In the early stages of developing production 3D, AM. printed equipment and materials, Bel Air was engaged by EOS to develop post processing techniques in order to feedback to the printing process for improvements to help post processing achieve traditional finishes.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.