Before Post-Processing

After Post-Processing

Objective
SLS Polypropylene secondary smoothing process
| Industry | 3d Print Post Process Tech – Plastic – Medical |
| Part Description | Medical Brace Printed Using FDM Technology |
| 3D Printing Technology | FDM |
| Material | Polypropylene |
| Process Technology | Smooth and polish surface |
| Equipment Type | High Energy |