Before Post-Processing

After Post-Processing

Objective
Additive Manufactured Plastic required a mirror like reflective surface
| Industry | 3D Printed Post Process – Plastics |
| Part Description | Additive Manufactured Product |
| 3D Printing Technology | Cleaning/Coating |
| Material | SLM |
| Process Technology | Standard Coating – Aluminizing |
| Equipment Type | Service Provider |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.