Before

As-printed 3D UV-acrylic gaming die showing a rough, cloudy surface before smoothing and polishing.

After

Smooth, transparent, high-clarity finish on a 3D-printed UV acrylic gaming die after high-energy disc finishing.

Objective

Automate the finishing of 3D-color-printed UV acrylic resin dice to achieve a clear, polished, consumer-ready surface. Improve transparency, remove print haze, and eliminate the need for manual sanding or hand polishing.

Industry3D Post-Processing – Plastic, Consumer Goods
Part DescriptionGame Dice – 3D Color
3D Printing TechnologySLA
MaterialUV Acrylic Resin
Process TechnologySmooth & Polish Surface
Equipment TypeHigh Energy Centrifugal Disc Finisher

Solution

Bel Air developed a high-energy centrifugal disc finishing process to refine and polish UV-cured acrylic resin dice printed on a Mimaki 3D color system. The as-printed parts exhibited surface haze, visible build lines, and reduced clarity.

Bel Air engineered an automated finishing method that:

  • Removes surface roughness and print texture
  • Restores transparency and color vibrancy
  • Produces a uniform gloss across all die faces
  • Eliminates manual sanding and hand polishing
  • Ensures repeatable quality for production-scale gaming dice

This automated process delivers a clear, polished, and consistent appearance suitable for premium game components while supporting efficient, scalable manufacturing.

If you are unsure what equipment and media you require to achieve your desired surface finish, send us your part, and we will evaluate it and provide you with a detailed metrology report.

To explore various achievable finishes, you can also request a comparative keychain sampleshowcasing a range of surface textures and polish levels.