Nylon SLS-printed consumer art, before post-processing.

Before

Nylon SLS-printed consumer art, after post-processing.

After

Objective

Enhance the surface finish of Nylon SLS-printed consumer art pieces for improved cosmetic appeal and product quality, achieving a polished, molded-like finish.

IndustryImprove Surface Finish
Part DescriptionConsumer Art
3D Printing Technology 3D Plastic SLS
Material Formiga P110
Process TechnologySmooth & Polish Surface
Equipment TypeIndustrial 3D Print Smoother

Solution

Bel Air Finishing collaborated with the customer to improve the surface finish of Formiga P110 nylon parts. Using the Industrial 3D Print Smoother, the process involved smoothing and polishing the surface to eliminate roughness typical of SLS printing. This water-based slurry system delivered a consistent, molded-like finish while preserving intricate design details.

By refining surface finishing techniques, Bel Air provided valuable insights to help the customer evaluate 3D printing technologies and post-processing methods. This solution ensures consumer art pieces meet high cosmetic and quality standards, supporting their use in premium applications.

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.