Objective
Evaluate process options
Industry | 3d Print Post Process Tech – Metal – Automotive |
Part Description | Turbine Impeller |
3D Printing Technology | DMLS |
Material | ALSi 10Mg Aluminum |
Process Technology | Evaluation of different process methods (3d) |
Equipment Type | High Energy |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.