Before

3d printed titanium medical implant, before

After

Objective

De-Powder and polish trial medical components.

Industry3D Print Post Process Tech –  Metal – Medical
Part DescriptionMedical Implant
3D Printing TechnologyEOS DMLS
MaterialTitanium TIAL4V
Process TechnologySmooth & Polish Surface. De-Powder.
Equipment TypeHigh Energy

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.