Before Post-Processing
After Post-Processing

Objective
Development to determine multiple process options
Industry | 3d Print Post Process Tech – Metal – Jewelry |
Part Description | Stainless steel ring |
3D Printing Technology | Metal – DMLS |
Material | 17-4 Stainless Steel |
Process Technology | Evaluation of Different Process Methods (3D) |
Equipment Type | Multiple Technologies |
In the early stages of developing production 3D, AM. printer equipment and materials, Bel Air was engaged with Jostens to develop post processing techniques in order to feedback to the printing process for improvements to help post processing achieve traditional finishes.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.