Before Post-Processing

After Post-Processing

Objective
Surface Polish
| Industry | 3d Print Post Process Tech – Metal |
| Part Description | Artwork |
| 3D Printing Technology | Metal – SLM |
| Material | Stratasys Stainless Steel 316 |
| Process Technology | Smooth and Polish surface |
| Equipment Type | High Energy |
In the early stages of developing production 3D, AM. printer equipment and materials, Bel Air was engaged with Stratasys to develop post processing techniques in order to feedback to the printing process for improvements to help post processing achieve traditional finishes.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.