Before

After

Objective
Internal Surface Finish Improvement
| Industry | 3D Print Post Process Tech – Metal |
| Part Description | Strainer |
| 3D Printing Technology | Metal – EOS DMLS |
| Material | Raw Metal 17-4 Stainless Steel |
| Process Technology | Surface and Polish Finish |
| Equipment Type | Proprietary |
With the advent of 3D or Additive Manufacturing metal printing technology printer manufacturers like EOS, as well as aerospace component manufactures have come to BAF to help develop process techniques to be able to understand the viability and or establish standardized processing that need to be adapted to compensate for the as printed roughness of multiple components, materials and geometries.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.