Objective
Bel Air Finishing was tasked with delivering a precision surface finishing and polishing solution for titanium medical implants. The goal is to achieve a smooth, machined finish that meets the high standards of the medical industry, allowing clients to optimize 3D printing technologies for titanium components and make informed decisions on post-processing techniques.
| Industry | 3d Print Post Process Tech – Metal – Medical |
| Part Description | Medical Bone Plate Implant |
| 3D Printing Technology | DMLS (OESINT M) |
| Material | Titanium Ti64 |
| Process Technology | Smooth and Polish Surface |
| Equipment Type | High Energy |
Solution
Bel Air developed a high-energy finishing solution using the Centrifugal Disc Finisher to precisely smooth and polish titanium bone plate implants. This process achieves a machined finish that meets stringent medical standards for durability and surface quality. Through rigorous testing and process development, we helped the customer achieve consistent, high-quality results that enhance the performance, longevity, and aesthetic appeal of 3D-printed titanium implants. By reducing the need for manual polishing, this solution also increases production efficiency, supporting the scalability of medical manufacturing.