Before Post-Processing


After Post-Processing


Objective
Bel Air completed testing of surface finishing and coating for the customer to help them make educated decisions to best choose the printing technologies. Titanium materials post processed to a machined finish.
Industry | 3d Print Post Process Tech – Metal – Medical |
Part Description | Medical Bone Plate Implant |
3D Printing Technology | DMLS (OESINT M) |
Material | Titanium Ti64 |
Process Technology | Smooth and Polish Surface |
Equipment Type | High Energy |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.