Before

After

Objective
DMLS Printed 17-4 stainless steel firearms components
| Industry | Firearms |
| Part Description | 3D Trigger |
| 3D Printing Technology | DMLS |
| Material | 17-4 Stainless Steel |
| Process Technology | De-Powder & Smooth Surface |
| Equipment Type | Water Jet Slurry Blast |
The customer wants to bring the very complicated geometry to a smooth and functional surface
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.