Before


After


Objective
Remove print layer lines from a 17-4 Stainless Steel BJ print Test Sample
| Industry | 3D Printed Metal Post Processing |
| Part Description | 3D Printed Test Bar |
| 3D Printing Technology | BinderJer |
| Material | 17-4PH Stainless Steel |
| Process Technology | Multiple Methods, Polish |
| Equipment Type | High Energy |
Customer requests that we run the part through a specific process that eliminates the printer layer lines on the 17-4PH Stainless test bar. This process will be achieved with a high energy solution such as the FMSL series of equipment.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.