Before Post-Processing

After Post-Processing

Objective
DMLS printed Titanium part for post-processing
Industry | 3D printed post process Metal – automotive |
Part Description | Paint Bell |
3D Printing Technology | DMLS/SLM |
Material | Titanium |
Process Technology | Smooth/Polish Surface |
Equipment Type | Multiple Technologies |
In the early sages of developing production 3D, Am printer equipment and materials, bel-air was engaged by GM to develop post processing techniques in order to feedback to the printer process for improvements to help post processing achieve traditional finishes.