Before Post-Processing


After Post-Processing


Objective
Improve Surface Finish
Industry | 3d Print Post Processing Tech – Metal |
Part Description | Medical Implant |
3D Printing Technology | Metal – DMLS |
Material | Titanium |
Process Technology | Smooth and polish surface |
Equipment Type | High Energy |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.