Before
After
Objective
Ultrapolish inconel sample as a feasibility.
Industry | 3D Print Post Process Tech – Metal – Aerospace |
Part Description | Aerospace Test Part |
3D Printing Technology | Metal – SLM |
Material | Inconel 718 |
Process Technology | Smooth & Polish Surface |
Equipment Type | High Energy |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.