Watch component after processing

Objective

Determine the optimum method to improve Surface Finish on Electrical Housings to suit the customer’s specific production and function.

Industry3D Printed Post Process – Plastics – Electronics
Part DescriptionElectronic Housings
3D Printing Technology3D Plastic MJF
MaterialHP PA 12
Process TechnologyEvaluation of Different Process Methods
Equipment TypeMultiple

In the early stages of developing production 3D AM Printer equipment and materials, Bel Air was engaged by HP (User) to develop post processing techniques in order to feed back to the printing process for improvements to help post processing achieve traditional finishes.

If you are unsure what equipment and media you require to achieve your desired surface finish, thenĀ send us your part, and we will evaluate it and provide you with a metrology report.