Objective

Improve surface finish to the feel of a molded part.

Industry3D Printing Plastics – Test Samples
Part Description Chess Piece
3D Printer Technology PA11
MaterialCarbon Fiber Composite
Process TechnologySmooth and Polish Surface
Equipment TypeHigh Energy

In the early stages of developing production 3D, AM. printer equipment and materials, Bel Air was engaged with EOS to develop post processing techniques in order to feedback to the printing process for improvements to help post processing achieve traditional finishes.

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.