Before Post-Processing

watch component before post-processing

After Post-Processing

Watch component after processing

Objective

Post-Process Polish

Industry3D Post Processing Tech – Metal – Consumer
Part Description3D Printed Art
3D Printing TechnologyExOne BJ Binder Jet
Material420 Stainless Steel – Bronze
Process TechnologySurface & Polish Surface + Evaluation of Different Process Methods (3D)
Equipment TypeHigh Energy

In the early stages of developing production 3D, AM. printer equipment and materials, Bel Air was engaged with ExOne to develop post processing techniques in order to feedback to the printing process for improvements to help post processing achieve traditional finishes.

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.