Before Post-Processing

After Post-Processing

Objective
Improve the surface finish of the Internal Passage fir functionality.
| Industry | 3D Print Post Process Tech – Metal – Automotive |
| Part Description | AM Automotive Parts |
| 3D Printing Technology | Metal – EBM |
| Material | 3D Steel Alloys |
| Process Technology | Smooth & Polish Surface |
| Equipment Type | 3D Water Jet Slurry Blaster |
In the early stages of developing production 3D, AM. printer equipment and materials, Bel Air was engaged with a customer to develop post processing techniques in order to feedback to the printing process for improvements to help post processing achieve traditional finishes.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.