Before Post-Processing

After Post-Processing

Objective
Surface finish improvement for feasibility study to see the effect on internal threads.
| Industry | 3D Print Post Process Tech – Metal – Aerospace |
| Part Description | AM Aerospace Part, Nut |
| 3D Printing Technology | Metal – DMSL |
| Material | 17-4 Stainless Steel |
| Process Technology | Smooth and Polish Finish |
| Equipment Type | High Energy |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.