Before

After

Objective
Improve Surface Finish
| Industry | 3D Printer Plastics – Medical |
| Part Description | Medical Implants |
| 3D Printer Technology | MJF |
| Material | HP PA 1100 |
| Process Technology | Smooth & Polish Surface |
| Equipment Type | Centrifugal Disc Finisher |
Bel Air completed testing of surface finishing an coating for the customer to help them make educated decisions to best choose the printing technologies. Nylon materials post processed to a molded finish.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.