Before Post-Processing

After Post-Processing

Objective
Improve surface finish, remove build lines.
| Industry | 3d Print Post Process Tech – Plastic – Test |
| Part Description | Fan |
| 3D Printing Technology | FDM |
| Material | ASA |
| Process Technology | Smooth and polish surface |
| Equipment Type | High Energy |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.