Before

After

Objective
Bel Air Finishing was tasked with demonstrating and evaluating surface finishing techniques for Binder Jet 17-4 stainless steel hardware components of various geometries. The goal was to explore multiple methods to achieve different levels of finish quality, addressing the inherent roughness of as-printed surfaces.
| Industry | 3D Printed Metal Post Processing |
| Part Description | Hardware of Various geometries |
| 3D Printing Technology | BinderJet |
| Material | 17-4 Stainless Steel |
| Process Technology | Evaluation of Different Process Methods |
| Equipment Type | High-Energy Centrifugal Disc Finisher, Industrial 3D Print Smoother |
Solution
To meet the needs of leading 3D printer manufacturers like Desktop Metal and aerospace component producers, Bel Air Finishing utilized the High-Energy Centrifugal Disc Finisher and the Industrial 3D Print Smoother. These advanced systems provided a range of surface preparation options, from smoothing to ultra-polishing, tailored to meet specific industry requirements.
Bel Air’s testing and evaluation process refined reliable and repeatable post-processing methods, ensuring consistent, high-quality results. This automated approach reduced manual labor, improved surface uniformity, and enabled manufacturers to meet stringent aerospace and industrial standards. By partnering with Bel Air, customers gained valuable insights into the best practices for finishing metal parts, optimizing their production workflows.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.