Objective
Replace Hand Sanding on casting models
Industry | 3D Printing Plastic – Aerospace |
Part Description | Aerospace Part |
3D Printer Technology | 3D Plastic SLA |
Material | SLA Resin |
Process Technology | Proprietary |
Equipment Type | Centrifugal Disc Finisher |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.