Before

After

Objective
Improve Surface Finish to molded quality for fit, form & function.
| Industry | 3D Printing Plastic – Test Samples |
| Part Description | Adjustable Wrench |
| 3D Printer Technology | FDM |
| Material | PLA |
| Process Technology | Smooth and Polish Surface |
| Equipment Type | High-Energy Centrifugal Disc Finisher |
Bel Air completed testing of surface finishing and coating for the customer to help them make educated decisions to best choose the printing technologies. PLA materials post processed to a molded finish.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.