Surface Finishing of 3D Metal Printed Parts
The following are examples of the various surface finishing recipes that we have developed. These can be used for all types of Additive Manufactured materials and technology types, including but not limited to the list below. Each picture indicates a different finishing process that used our equipment and abrasive/polishing media. The roughness average (Ra) is measured in micro-inches. These finishes are industry standard for each material, but we also develop custom finishing recipes to meet your specifications. Let us process your samples and find a result that is right for you.
Surface Finishing: EOS DMLS
DMLS Printed Stainless Steel – Standard Degrees of Finish
The following are examples of Direct Metal Laser Sintering (DMLS) printed parts. Each picture indicates a different finishing process that used our equipment and abrasive/polishing media. The roughness average (Ra) is measured in micro-inches. These finishes are industry standard, but we also develop custom finishing recipes to meet your specifications.
Surface Finishing: EOS DMLS
DMLS Printed 17-4 Stainless Steel – Standard Degrees of Finish
Surface Finishing: Arcam/GE EBM
EBM Printed Titanium 6AL4V ELI – Standard Degrees of Finish
The following are examples of Electron Beam Melting (EBM) printed parts. Each picture indicates a different finishing process that used our equipment and abrasive/polishing media. The roughness average (Ra) is measured in micro-inches. These finishes are industry standard , but we also develop custom finishing recipes to meet your specifications.
Surface Finishing: Markforged Metal FFF
Markforged Metal FFF 17-4PH Stainless Steel Alloy –
Standard Degrees of Finish
As Printed

Process WJ


Process A-1


Process R-2


Process B-2


Process C-2


Surface Finishing: ExOne Binder Jet
Binder Jet Printed 316L Stainless Steel – Standard Degrees of Finish
The following are examples of Binder Jet (BJ) printed parts. Each picture indicates a different finishing process that used our equipment and abrasive/polishing media. The roughness average (Ra) is measured in micro-inches. These finishes are industry standard, but we also develop custom finishing recipes to meet your specifications.