Electroplating

Electroplating 3D Printed Parts

Bel Air’s state-of-the-art electroplating facility provides depositions of copper (Cu), nickel (Ni), silver (Ag), Gold (Au), and Palladium (Pd). Electroplating may or may not be applied to parts that have previously been surface finished using one of the processes shown in the Surface Finishing section. The examples below indicate the general range of plating currently available (note that the first letter in the designation indicates the pre-finish before coating).

Electroplating Samples: Plastic

The following are examples of 3D-printed plastic parts that have gone through various post-processes before electroplating. The electroplating shown are Copper plating as printed, Copper Pre-Finish after Process C, Nickel plated as printed, Nickel Pre-Finish after Process C, and Gold 24KT after Process C.

Copper,

Raw

(RCu)

3D printed plastic part, copper plated, raw form

Copper,

Pre-Finish

(CCu)

Copper plated, finished, 3D printed plastic part

Nickel

Raw

(RNi)

3D printed part, nickel plated, raw form

Nickel

Raw

(RNi)

3D printed part, nickel plated, raw form

Nickel,

Pre-Finish

(CNi)

3D printed plastic part, nickel plated, finished form

Gold,

24KT

(CAu)

Electroplating sample

Electroplating Samples: Metal & Plastic

The following are examples of 3D-Printed metal and plastic parts before and after they have gone through the electroplating process.

17-4 SS

Steel Polish

3D printed stainless steel part that has been polished

24K

Gold Plate

3D Printed Metal Part, 24k Gold Plated

DMLS SS

Steel Pre-Plate

3D printed metal part in pre-plated form

DMLS SS

Steel Plated

Plated, 3D printed metal part

718 SS

Steel Polish

718 SS ring before

24K

Gold Plate

718 SS ring after plating

PA12 Nylon

Printed

PA12 brain as printed

24k

Gold Plated

PA12 brain gold plated

Physical Vapor Deposition (PVD)

Physical Vapor Deposition is typically used for high-wear applications and in any industry where the visual and functional performance of an item can be enhanced with a durable decorative coating. For example, PVD coatings are commonly used in automotive, plumbing, hardware manufacturing, medical, and electronic applications as well as for large and multi-dimensional parts.

Stainless Steel

Pre-Coating

Color coding of dental tools

Stainless Steel

Post Coating

pvd coated metal