Wet Blasting Equipment: WaterJet

A wet surface treatment process which cleans, descales, and degreases in a single operation without chemicals or solvents. A pressurized blasting mixture of water and abrasive media treats the part surface by scrubbing rather than impinging and impact, without changing close tolerance dimensions. The pressure blast process is the preferred method or preparing metal, plastic, and composite surfaces in the numerous industries, such as: Aerospace, Plating, Electronics, and more!

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it free-of-charge and provide you with a metrology report.

FM-WJ Tabletop Models

Bel Air's Mini Water Jet Blaster

Available Models

  • FM-WJ Mini
  • FM-WJ Mini-T

Standard Features

  • All welded stainless steel construction
  • Safety interlock blast system
  • Large view window with foot-operated wash
  • Filtered cabinet exhaust system
  • Regulator w/gauge for variable air pressure
  • Suction gun & pump gun system available
  • Fluorescent lighting of cabinet interior
  • Coated Interior work table
  • Water rinse & air blow off nozzle included

Automation Options

  • Turntable – Manual or motorized. Built in or removable. Available in sizes ranging from 12″ diameter to 72″ diameter
  • Tumble Basket– Automated batch processing for powder removal

FM-WJ Floor Models

water jet blaster designed for post processing 3D printed parts

Available Models

  • FM-WJ33-1
  • FM-WJ33-2
  • FM-WJ36-2
  • FM-WJ45-2
  • FM-WJ65-2

Standard Features

  • All welded stainless steel construction
  • Safety interlock blast system
  • Large view window with foot-operated wash
  • Filtered cabinet exhaust system
  • Regulator w/gauge for variable air pressure
  • Suction gun & pump gun system available
  • Fluorescent lighting of cabinet interior
  • Coated Interior work table
  • Water rinse & air blow off nozzle included

Automation Options

  • Turntable – Manual or motorized. Built in or removable. Available in sizes ranging from 12″ diameter to 72″ diameter
  • Tumble Basket– Automated batch processing for powder removal

Product Comparison Table

ModelDimensions (D x W x H)Door OpeningTotal Air ConsumptionElectricalSuctionPressureBasket
FM-WJ Mini24″ X 20″ X 24″10 X 1240-60 cfm
@ 80 psi
115v✔N/AN/A
FM-WJ Mini-T30″ X 20″ X 24″10 X 1240-60 cfm
@ 80 psi
115v✔N/A✔
FM-WJ33-133″ X 33″ X 92″22 X 2240-60 cfm
@ 80 psi
115v/220v✔N/AOptional
FM-WJ33-233″ X 33″ X 92″22 X 2240-60 cfm
@ 80 psi
115v/220v✔✔Optional
FM-WJ36-236″ X 36″ X 92″24 X 2440 cfm
@ 80 psi
115v/220v✔✔Optional
FM-WJ45-250″ X 40″ X 103″29 X 2940 cfm
@ 80 psi
115v/220v✔✔Optional
FM-WJ65-260″ X 50″ X 104″40 X 4040 cfm
@ 80 psi
115v/220v✔✔Optional

Wet Blasting vs Dry Blasting Comparison Table

FEATUREWET BLASTINGDRY BLASTING
Good for Delicate Partsplusplus
Preserve Details on Intricate Partsplusminus
Precision Surface Smoothingplusminus
Dust-Free/Cleanroom Friendlyplusdouble minus
Surface Uniformityplusplus
Component Deburringdouble plusplus
Component Descalingplusplus
Component Cleaningdouble plusminus
Internal Finishingplusdouble minus
Component Peeningminusplus

Sample Work