Objective
Improve Surface Finish & Dye
| Industry | 3D Printing Plastic – Test Samples |
| Part Description | Display Tags |
| 3D Printer Technology | SLS |
| Material | PA – 1200 |
| Process Technology | Dying Additive Manufactured Parts |
| Equipment Type | Coating Equipment |
Bel Air completed testing of surface finishing and coating for the customer to help them make educated decisions to best choose the printing technologies. Pa-1200 materials post process to a molded finish.
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.